Takayuki Narushima
Takayuki Narushima
Email yang diverifikasi di material.tohoku.ac.jp - Beranda
JudulDikutip olehTahun
High‐temperature passive oxidation of chemically vapor deposited silicon carbide
T Narushima, T Goto, T Hirai
Journal of the American Ceramic Society 72 (8), 1386-1390, 1989
1941989
High-temperature oxidation of silicon carbide and silicon nitride
T Narushima, T Goto, T Hirai, Y Iguchi
Materials transactions, JIM 38 (10), 821-835, 1997
1401997
High‐Temperature Active Oxidation of Chemically Vapor‐Deposited Silicon Carbide in an Ar─O2 Atmosphere
T Narushima, T Goto, Y Iguchi, T Hirai
Journal of the American Ceramic Society 74 (10), 2583-2586, 1991
1011991
High‐temperature oxidation of chemically vapor‐deposited silicon carbide in wet oxygen at 1823 to 1923 K
T Narushima, T Goto, Y Iguchi, T Hirai
Journal of the American Ceramic Society 73 (12), 3580-3584, 1990
971990
Japanese research and development on metallic biomedical, dental, and healthcare materials
M Niinomi, T Hanawa, T Narushima
JOM 57 (4), 18-24, 2005
762005
The Wulff shape of Alumina: II, experimental measurements of pore shape evolution rates
M Kitayama, T Narushima, AM Glaeser
Journal of the American Ceramic Society 83 (10), 2572-2583, 2000
732000
Preparation of calcium phosphate films by radiofrequency magnetron sputtering
T Narushima, K Ueda, T Goto, H Masumoto, T Katsube, H Kawamura, ...
Materials transactions 46 (10), 2246-2252, 2005
632005
The Wulff shape of alumina: I, modeling the kinetics of morphological evolution
M Kitayama, T Narushima, WC Carter, RM Cannon, AM Glaeser
Journal of the American Ceramic Society 83 (10), 2561-2531, 2000
592000
High‐Temperature Active Oxidation of Chemically Vapor‐Deposited Silicon Carbide in CO─CO2 Atmosphere
T Narushima, T Goto, Y Yokoyama, Y Iguchi, T Hirai
Journal of the American Ceramic Society 76 (10), 2521-2524, 1993
541993
Oxygen solubility in liquid silicon
T Narushima, K Matsuzawa, Y Mukai, Y Iguchi
Materials Transactions, JIM 35 (8), 522-528, 1994
511994
Carbide formation and dissolution in biomedical Co-Cr-Mo alloys with different carbon contents during solution treatment
S Mineta, S Namba, T Yoneda, K Ueda, T Narushima
Metallurgical and materials transactions A 41 (8), 2129-2138, 2010
502010
Precipitates in biomedical Co-Cr alloys
T Narushima, S Mineta, Y Kurihara, K Ueda
Jom 65 (4), 489-504, 2013
442013
Hydrothermal synthesis of zeolite A using blast furnace slag
Y Sugano, R Sahara, T Murakami, T Narushima, Y Iguchi, C Ouchi
ISIJ international 45 (6), 937-945, 2005
412005
Solubility of carbon in liquid silicon equilibrated with silicon carbide
K Yanaba, M Akasaka, M Takeuchi, M Watanabe, T Narushima, Y Iguchi
Materials Transactions, JIM 38 (11), 990-994, 1997
411997
Fabrication of calcium phosphate films for coating on titanium substrates heated up to 773 K by RF magnetron sputtering and their evaluations
K Ueda, T Narushima, T Goto, M Taira, T Katsube
Biomedical Materials 2 (3), S160, 2007
402007
Advances in Metallic Biomaterials
M Niinomi, T Narushima, M Nakai
Heidelberg, DE: Springer, 2015
372015
Oxidation or nitridation behavior of pure chromium and chromium alloys containing 10 mass% Ni or Fe in atmospheric heating
K Taneichi, T Narushima, Y Iguchi, C Ouchi
Materials transactions 47 (10), 2540-2546, 2006
372006
Microstructures, mechanical properties and cytotoxicity of low cost beta Ti–Mn alloys for biomedical applications
PF Santos, M Niinomi, K Cho, M Nakai, H Liu, N Ohtsu, M Hirano, M Ikeda, ...
Acta biomaterialia 26, 366-376, 2015
342015
Effects of niobium ions released from calcium phosphate invert glasses containing Nb2O5 on osteoblast-like cell functions
A Obata, Y Takahashi, T Miyajima, K Ueda, T Narushima, T Kasuga
ACS applied materials & interfaces 4 (10), 5684-5690, 2012
342012
Titanium and its alloys as biomaterials
T Narushima
J. Jpn. Inst. Light Metals 55, 561-565, 2005
322005
Sistem tidak dapat melakukan operasi ini. Coba lagi nanti.
Artikel 1–20